60s/2/3 sewing thread for clothes bags and leathers
We are professional manufacturer of polyester sewing thread
Our factory covers an area over 75,000 square meters ,with 200,000 spindles ,and a monthly output 2000tons .
Equipped with the advanced auto machine in air conditioned workshops ,and advanced testing laboratory and strickly QA management .
We also have skilled and experienced workers ,professional management team .
Our main products spun polyester yarn 20s/2/3 to 80s/2/3 and poly poly core yarn 12s/2/3 to 60s/2/3 .
From year 2021 ,our company also developed polyester high tenacity yarn .
Guided by the principle of "Quality first ,credibility first and sincere service " .Our aim at "winning by quality ,customer first,and integrity management " ,Our aim is to be the benchmark in polyester sewing thread industry ; we tak customers' affirmation of our service and quality as the source of our efforts .
If you have any enquiry ,please feel free to contact with us .thank you!
STANDARD QUALITY FOR SEWING THREAD SSP | ||||||||||
ITEM | DENSITY ( g/CM 3 ) | DENIER ( d ) | TWIST ( t/m ) | STRENGTH ( gf ) | ELONGATION ( % ) | |||||
AVERAGE | MIN - MAX | AVERAGE | MIN - MAX | AVERAGE | MIN - MAX | AVERAGE | MIN - MAX | AVERAGE | MIN - MAX | |
20s/2 | 0.41 | 0.39 - 0.44 | 525 | 500 - 550 | 575 | 550 - 600 | 2125 | 2020 | 14 | 12 - 16 |
20s/3 | 0.41 | 0.39 - 0.44 | 775 | 745 - 805 | 540 | 525 - 555 | 3400 | 3100 | 15 | 12 - 18 |
30s/2 | 0.41 | 0.39 - 0.44 | 360 | 350 - 370 | 750 | 720 - 770 | 1350 | 1200 | 16 | 12 - 16 |
40s/2 | 0.41 | 0.39 - 0.44 | 265 | 250 - 280 | 805 | 765 - 850 | 1065 | 1010 | 14 | 12 - 16 |
40s/3 | 0.41 | 0.39 - 0.44 | 400 | 380 - 420 | 680 | 645 - 715 | 1595 | 1520 | 14 | 12 - 16 |
45s/2 | 0.41 | 0.39 - 0.44 | 236 | 210- 245 | 832 | 779 -864 | 970 | 920 | 13 | 11-16 |
50s/2 | 0.41 | 0.39 - 0.44 | 210 | 200 - 225 | 960 | 910 - 1010 | 850 | 810 | 14 | 12 - 16 |
50s/3 | 0.41 | 0.39 - 0.44 | 315 | 295 - 335 | 780 | 755 - 805 | 1350 | 1180 | 14 | 12 - 16 |
60s/2 | 0.41 | 0.39 - 0.44 | 175 | 165 - 185 | 990 | 960 - 1020 | 700 | 620 | 12 | 10 - 14 |
60s/3 | 0.41 | 0.39 - 0.44 | 265 | 250 - 280 | 880 | 855 - 905 | 1100 | 960 | 13 | 11- 15 |
STANDARD QUALITY FOR POLY POLY CORE YARN | |||||||||
ITEM | DENSITY ( g/CM 3 ) | DENIER ( d ) | TWIST ( t/m ) | STRENGTH ( gf ) | ELONGATION ( % ) | ||||
AVERAGE | MIN - MAX | AVERAGE | MIN - MAX | AVERAGE | MIN - MAX | MIN - MAX | AVERAGE | MIN - MAX | |
20S/2 | 0.41 | 0.39 - 0.44 | 635 | 625-655 | 500 | 470-530 | 3750 | 17 | 16-18 |
29S/2 | 0.41 | 0.39 - 0.44 | 380 | 370-395 | 705 | 670-745 | 1980 | 18 | 16-20 |
37S/2 | 0.42 | 0.39 - 0.42 | 295 | 280-310 | 600 | 570-630 | 1750 | 18 | 16-20 |
45S/2 | 0.41 | 0.39 - 0.44 | 240 | 230-255 | 980 | 930-1030 | 1400 | 18 | 16-20 |
60S/2 | 0.41 | 0.39 - 0.44 | 175 | 170-185 | 957 | 910-1005 | 900 | 15 | 13-17 |
PPC Strength report | |||||||||
Test temperature:23 | Yarn count :12S/2 | Tension :0.05 CN/dtex | |||||||
Test speed :1300mm/min | Test humidity:66% RH | Nominal fineness:976 dtex | |||||||
Number of times | Average | variance | CV | Q (95%) | Min | Max | |||
Break strength (CN/dtex) | 10 | 5.02 | 0.1 | 2.06 | 0.07 | 4.83 | 5.11 | ||
Breaking strength (CN) | 10 | 4902.8 | 100.91 | 2.06 | 72.12 | 4715 | 4984.8 | ||
Elongation | 10 | 21.34 | 0.65 | 3.05 | 0.46 | 20.19 | 21.89 | ||
Breaking time | 10 | 4.96 | 0.15 | 3.08 | 0.11 | 4.69 | 5.09 | ||
Fracture work(CN.CM) | 10 | 264.66 | 15.05 | 5.69 | 10.76 | 236.53 | 278.59 |
PPC Strength report | |||||||||
Test temperature:20 | Yarn count :16S/2 | Tension :0.05 CN/dtex | |||||||
Test speed :1300mm/min | Test humidity:65% RH | Nominal fineness:729 dtex | |||||||
Number of times | Average | variance | CV | Q (95%) | Min | Max | |||
Break strength (CN/dtex) | 5 | 5.7 | 0.07 | 1.19 | 0.09 | 5.6 | 5.77 | ||
Breaking strength (CN) | 5 | 4155.4 | 49.56 | 1.19 | 61.61 | 4085.2 | 4205.4 | ||
Elongation | 5 | 20.75 | 0.55 | 2.64 | 0.68 | 19.97 | 21.46 | ||
Breaking time | 5 | 4.83 | 0.13 | 2.73 | 0.16 | 4.64 | 5 | ||
Fracture work(CN.CM) | 5 | 214.38 | 9.99 | 4.66 | 12.43 | 199.52 | 224.44 |
PPC Strength report | |||||||||
Test temperature:20 | Yarn count :20S/2 | Tension :0.05 CN/dtex | |||||||
Test speed :1300mm/min | Test humidity:65% RH | Nominal fineness:588 dtex | |||||||
Number of times | Average | variance | CV | Q (95%) | Min | Max | |||
Break strength (CN/dtex) | 10 | 5.43 | 0.08 | 1.54 | 0.06 | 5.3 | 5.56 | ||
Breaking strength (CN) | 10 | 3190.9 | 49 | 1.54 | 35.02 | 3119.2 | 3266.4 | ||
Elongation | 10 | 19.92 | 0.49 | 2.49 | 0.35 | 19.46 | 20.73 | ||
Breaking time | 10 | 4.64 | 0.11 | 2.48 | 0.08 | 4.53 | 4.83 | ||
Fracture work(CN.CM) | 10 | 157.09 | 7.22 | 4.6 | 5.16 | 147.44 | 168.8 |
21S/2 | 21S/3 | 21S/4 | 40S/2 | 50S/2 | 50S/3 | ||
1. Sizing | (Dtex) | 562.3 | 843.5 | 1124.76 | 295.25 | 236.2 | 354.3 |
count(Ne) | 21.5s/2 | 21.3s/3 | 21.2s/4 | 40.3s/2 | 50.7s/2 | 50.1s/3 | |
cv % of Count | 1.06 | 0.93 | 0.61 | 0.49 | 0.75 | 0.79 | |
Avg. Moisture Content % | |||||||
Corrected (Dtex) | 549.3 | 831.69 | 1111.42 | 293.05 | 232.93 | 353.59 | |
2. Twist | Twist per meter(TPM) | 578 | 483 | 437 | 825 | 897 | 784 |
Twist per inch(Tpi) | 14.68 | 12.26 | 11.09 | 20.95 | 22.78 | 19.91 | |
Cv % of Tpi | 1.37 | 0.81 | 2.3 | 1.2 | 1.5 | 1 | |
Twist Direction | S | S | S | S | S | S | |
3. Strength | Breaking Load (cN) | 2148 | 3647 | 1079 | 850 | 1343 | |
CV % of Breaking Load | |||||||
Elongation % | 17.87 | 19.4 | 15.8 | 15.27 | 17.4 | ||
Tenacity(cN/Tex) | 40.12 | 41.43 | 36.8 | 36.07 | 37.98 | ||
Sewable Faults(FTK) | 1 | 0.4 | 0 | 1.3 | 0.4 | 0 | |
4. Imperfection | Non-Sewable Faults(FTK) | 0 | 0 | 0 | 0 | 0 | 0 |
Total faults (FTK) | 2.5 | 2.9 | 1.2 | 3.3 | 4.2 | 1.3 | |
5. Shrinkage % | (Dry Heat) | 1.5 | 1.5 | 1.5 | 1 | 1 | 1 |
6. Density | (gm/cc) | 0.39-0.42 | 0.39-0.42 | 0.39-0.42 | 0.39-0.42 | 0.39-0.42 | 0.39-0.42 |
7. Hairiness Index % | 2.55 | 2.54 | 0.9 | 1.8 | 2.98 | 3.25 |
COUNTS | PRODUCT USAGE |
20S/2
|
Jeans,shoes,caps,leather products,etc.
|
20S/3
|
Jeans,shoes,handbags,leather products,etc.
|
20S/4
|
Packing bags,leather products,handbags,shoes,etc.
|
20S/6
|
Packing bags,canvas
|
20S/9
|
Jeans,handbags,leather products
|
30S/2
|
Suits,Bedcover, Bedsheet Sportwear,Notions ,Sweing craft and notions,etc
|
30S/3
|
Tents,Jeans,Leather products,Shoes, Baby clothes.
|
40S/2
|
Suits, Bedcover, Bedsheet, Sportwear,Notions,Sweing craft and notions,etc
|
50S/2
|
Knitting garments, ,Blouses, Suit-dress,Silks,Underwear,etc.
|
60S/2
|
Knitting garments,Suit-dress,overlooking thread,handketchief,underwear
|